Properties:
1. Green Flame
2. High mechanical strength
3. High temperature resistance
4. Good electrical performance
5. Totally made of virgin Material
SPECIFICATION:
Testing Condition
|
23±2°C, 50±5%RH
|
Test Project
|
Test Methods
|
Unit
|
Typical Values
|
Tensile Stress
|
GB/T1040-92
|
Mpa
|
≥95
|
Flexural Stress
|
GB/T 9341-2000
|
Mpa
|
≥140
|
Flexural Modulus
|
GB/T9341-2000
|
Mpa
|
≥5000
|
Impact Strength
|
GB/T1043-93
|
KJ/m2
|
≥8.0
|
Elongation At Break
|
GB/T1040-92
|
%
|
≥15
|
Heat Distortion Temperature
|
GB/T1634-2004
|
°C
|
≥200
|
MFR
|
GB/T 3682-2000
|
g/10min
|
8-20
|
Flame retardancy
|
GB/T 2408-1996
|
|
V-0
|
[1] Dyes materials characters will be different from above value.
[2] Typical values are for average laboratory data. It is only suit for utilizing reference, not on products standard.
ies
Application:
injection moulding; home componets; coilframe; lighting; linker
Package: Net weight 25.0 kg per bags.Coextruded paper bags lined with polyethylene film bags.
Test item |
Test condition |
Test method |
Test result |
Unit |
Physical propeties |
|
|
|
|
Density |
|
ASTM D792 |
1.55 |
g/cm 3 |
Water absorption |
saturation, 23 °C |
ASTM D570 |
0.6 |
% |
Molding shrinkage |
|
ASTM D955 |
0.3-0.5 |
% |
Glass fiber content |
|
ASTM D2117 |
30 |
% |
Melting Index |
250 °C ,5KG |
ASTM D1238 |
10 |
g/10min |
Mechanical properties |
|
|
|
|
Tensile strength |
23 °C ,DAM |
ASTM D638 |
120 |
Mpa |
Tensile elongation |
23 °C ,DAM |
ASTM D638 |
30 |
% |
Flexural strength |
23 °C ,DAM |
ASTM D790 |
180 |
Mpa |
Flexural modulus |
23 °C ,DAM |
ASTM D790 |
7800 |
Mpa |
Notched Izod impact(1/8") |
23 °C ,DAM |
ASTM D256 |
9.5 |
KJ/m 2 |
Thermal properties |
|
|
|
|
Deflection temperature |
1.82Mpa |
ASTM D648 |
215 |
°C |
Melting point |
|
ASTM D2117 |
- |
°C |
Flammability |
|
UL 94 |
HB |
- |
Machining parameters |
|
|
|
|
Drying temperature |
|
- |
100 |
°C |
Drying time |
|
- |
4 |
hr |
Processing temperature |
|
- |
235-255 |
°C |
Remarks |
30% Glass fiber reinforced |